| Title | Year |
| ANSI/AWS D8.8M-1997 SPECIFICATION FOR AUTOMOTIVE AND LIGHT TRUCK COMPONENTS WELD QUALITY—ARC WELDING (HISTORICAL) | 1997 |
| API-M:2006 STUDY GUIDE FOR API STANDARD 1104 - WELDING OF PIPELINES AND RELATED FACILITIES - TWENTIETH EDITION (HISTORICAL) | 1998 |
| B1.10: 1999 GUIDE FOR THE NONDESTRUCTIVE EXAMINATION OF WELDS (HISTORICAL) | 1999 |
| B1.11: 1988 GUIDE FOR THE VISUAL EXAMINATION OF WELDS (AWS B1.11) (HISTORICAL) | 1988 |
| B2.1-003: 1990 (SWPS) FOR GAS METAL ARC WELDING OF GALVANIZED STEEL, 10 THROUGH 18 GAGE, IN THE AS-WELDED CONDITION, (HISTORICAL) | 1999 |
| B2.1-1-015: (HISTORICAL) 1991 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL (M-1/P-1/S-1, GROUP 1 or 2), 1/8 THROUGH 1-1/2 INCH THICK, E7018, AS-WELDED OR PWHT CONDITION SITE LICENSE | 1991 |
| B2.1-1-027: 1998 STANDARD WELDING PROCEDURE SPECIFICATION(WPS) FOR; SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL(M-1/P-1/S-1, GROUP 1 OR 2),1/8 THROUGH 1/2 INCH THICK, E71T-11, AS-WELDED CONDITION | 1998 |
| B2.1-1-210: 2001 STANDARD WELDING PROCEDURE SPECIFICATION(WPS) FOR; GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERTS OF CARBON STEEL(M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, INMS-1 AND ER70S-2, AS-WELDED OR PWHT CONDITION(PRIMARILY PI | 2001 |
| B2.1-1-211: 2001 (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METALARC WELDING OF CARBON STEEL(M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUG1-1/2 INCH THICK, INMS-1, ER70S-2, AND | 2001 |
| B2.1-22-015: 2002 (SWPS) FOR; GAS TUNGSTEN ARC WELDING OF ALUMINUM (M/P/S-22 TO M/P/S-22), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING; SITE LICENSE (HISTORICAL) | 2002 |
| B2.1-4-217: 1999 (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CHROMIUM - MOLYBDENUM STEEL (M-4/P-4, GROUP 1 or 2), ER80S-B2, 1/8 THROUGH 1/2 IN. THICK, AS-WELDED CONDITION, 1/8 THROUGH 3/4 IN. THICK, (HISTORICAL) | 1999 |
| B2.1-4-218: 1999 (SWPS) FOR SHIELDED METAL ARC WELDING OF CHROMIUM - MOLYBDENUM STEEL (M-4/P-4, GROUP 1 or 2), E8018-B2, 1/8 THROUGH 1/2 IN. THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 in. THICK, PWHT CONDITION (HISTORICAL) | 1999 |
| B2.1-4-219: 1999 (SWPS) FOR; GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CHROMIUM- MOLYBDENUM STEEL(M-4/P-4, GROUP 1 OR 2), 1/8 THROUGH 1/2 IN.THICK,AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 IN.THIC (HISTORICAL) | 1999 |
| B2.1-4-220: 1999 (SWPS) FOR; GAS TUNGSTEN ARC WELDING(CONSUMABLE INSERT ROOT) OF CHROMIUM-MOLYBDENUM STEEL (M-4/P-4, GROUP 1 OR 2), 1/8 THROUGH 1/2 IN. THICK, AS- WELDED CONDITION, 1/8 THROUGH 3/4 IN.THICK, P (HISTORICAL) | 1999 |
| B2.1-4-221: 1999 (SWPS) FOR; GAS TUNGSTEN ARC WELDING(CONSUMABLE INSERT ROOT) FOLLOWED BY SHIELDED METAL ARCWELDING OF CHROMIUM-MOLYBDENUM STEEL(M-4/P-4, GROUP 1 OR 2), 1/8 THROUGH 1/2 IN.THICK, AS-WELDED CONDITION, 1/ (HISTORICAL) | 1999 |
| B2.1-5A-222: 1999 (SWPS) FOR; GAS TUNGSTEN ARC WELDING OF CHROMIUM-MOLYBDENUM STEEL(M-5A/P-5A), ER90S-B3, 1/8THROUGH 1/2 IN. THICK, AS-WELDED CONDITION, 1/8 THROUGH 3/4 IN. THICK, PWHT CONDITION, PRIMARILY PIPE APPLICA (HISTORICAL) | 1999 |
| B2.1-5A-223: 1999 (SWPS) FOR; SHIELDED METAL ARC WELDING OF CHROMIUM-MOLYBDENUM STEEL(M-5A/P-5A), E9018-B3, 1/8THROUGH 1/2 IN. THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 IN. THICK, PWHT CONDITION, PRIMARILY PIPE APP (HISTORICAL) | 1999 |
| B2.1-5A-224: 1999 (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CHROMIUM- MOLYBDENUM STEEL(M-5A/P-5A), 1/8 THROUGH 1/2 IN. THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 IN. THICK, PWHT (HISTORICAL) | 1999 |
| B2.1-5A-225: 1999 (SWPS) FOR GAS TUNGSTEN ARC WELDING(CONSUMABLE INSERT ROOT) OF CHROMIUM-MOLYBDENUM STEEL (M-5A/P-5A), 1/8 THROUGH 1/2 IN. THICK, AS-WELDED CONDITION, 1/8 THROUGH 3/4 IN. THICK, PWHT CONDITION, IN521 (HISTORICAL) | 1999 |
| B2.1-8-024: 2001 (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER3XX, AS-WELDED CONDITION, PRIMARILY PLATE AND STRUCTURAL APPLICATIONS | 2001 |
| B2.1-8-025: 2001 (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION, PR | 2001 |
| B2.1-8-212: 2001 (SWPS) FOR; GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER3XX, AS-WELDED CONDITION, PRIMARILY PIPE APPLICATIONS | 2001 |
| B2.1-8-213 1997 (SWPS) FOR; SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, E3XX-XX, AS-WELDED CONDITION (HISTORICAL) | 1997 |
| B2.1-8-213: 1997(R2007) (SWPS) FOR SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, E3XX-XX, AS-WELDED CONDITION (PRIMARILY PIPE APPLICATIONS) | 1997 (2007) |
| B2.1-8-214: 2001 (SWPS) FOR; GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION, PR | 2001 |
| B2.1-8-215: 2001 STANDARD WELDING PROCEDURE SPECIFICATION(WPS) FOR; GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT OF AUSTENITIC STAINLESS STEEL (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX AND ER3XX, AS-WELDED CONDITION(PRIMARILY PIPE | 2001 |
| B2.1-8-216: 2001 (SWPS) FOR GAS TUNGSTEN ARC WLEDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METALARC WELDING OF AUSTENITIC STAINLESS STEEL(M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX, ER3XX, A | 2001 |
| B2.1-BMG:2005 (HISTORICAL) Base Metal Grouping for Welding Procedure and Performance Qualification | 2005 |
| B2.1/B2.1-BMG: 2009 - BASE METAL GROUPING FOR WELDING PROCEDURES AND PERFORMANCE QUALIFICATIONS | 2009 |
| B2.1: 2005 SPECIFICATION FOR WELDING PROCEDURE AND PERFORMANCE QUALIFICATION (HISTORICAL) | 2005 |
| B2.2:1991 BRAZING PROCEDURE AND PERFORMANCE QUALIFICATION (HISTORICAL) | 1991 |
| B2.3/B2.3M:2008 SPECIFICATION FOR SOLDERING PROCEDURE AND PERFORMANCE QUALIFICATION | 2008 |
| B3.0: 1977 WELDING PROCEDURE AND PERFORMANCE QUALIFICATION (HISTORICAL) | 1977 |
| B4.0: 1998 STANDARD METHODS FOR MECHANICAL TESTING OF WELDS (US CUSTOMARY UNITS) (HISTORICAL) | 1998 |
| B4.0M: 2000 STANDARDS METHODS FOR MECHANICAL TESTING OF WELDS (METRIC CUSTOMARY UNITS) (HISTORICAL) | 2000 |
| B5.15:2003-AMD 1 - SPECIFICATION FOR THE QUALIFICATION OF RADIOGRAPHIC INTERPRETERS | 2003 |
| B5.17:2004 SPECIFICATION FOR THE QUALIFICATION OF WELDING FABRICATORS (HISTORICAL - PHOTOCOPY) | 2004 |
| B5.1:2003 (ERRATA 2007) SPECIFICATION FOR THE QUALIFICATION OF WELDING INSPECTORS | 2003 |
| B5.5:2000 SPECIFICATION FOR THE QUALIFICATION OF WELDING EDUCATORS | 2000 |
| BHC1 - BASICS OF BRAZING | 2007 |
| BRH: 1991 BRAZING HANDBOOK 4th EDITION | 1991 |
| BUNDLE A: 2006 | 2006 |
| BUNDLE A:2009 | 2009 |
| BUNDLE B: 2006 | 2006 |
| BUNDLE B: 2007 | 2007 |
| BUNDLE B:2009 | 2009 |
| BUNDLE C:2009 | 2009 |
| BUNDLE D:2008 | 2008 |
| C1.1M/C1.1:2000(R2006) RECOMMENDED PRACTICES FOR RESISTANCE WELDING | 2006 |